HY (Shanghai) Industry Co., Ltd.
Main products:Nickel Alloy Wire,Nickel Alloy Bar,Special Alloy,Electricity Heating Wire,Alloy Structure Steel
Products
Contact Us
  • Contact Person : Ms. Chen Grace
  • Company Name : HY (Shanghai) Industry Co., Ltd.
  • Tel : 0086-021-52286112
  • Fax : 0086-021-52286112-802 Address: Room 202, No.34, 155 Nong South Lian hua Rd, Minhang District, Shanghai, China Zip: 200237 Country/Region: China (Mainland) Province/State: Shanghai
  • Address : Shanghai,ShangHai,Room 202, No.34, 155 Nong South Lian hua Rd, Minhang District, Shanghai, China
  • Country/Region : China
  • Zip : 200237

Superalloy

Superalloy
Product Detailed
(Heat-resisting Superalloy Anticorrosion Alloy) Forged bar Size: 50-305mm Application: nuclear energy, aviation, spaceflight

Hastelloy B Chemical compostion:

Alloy 

%

Ni 

Mo 

Fe 

Cr 

Co 

Mn 

V

Si 

P

Hastelloy B

Min. 

Balance 

26

4

    

0.2

   

Max. 

30

6

1

2.5

0.05

1

0.4

1

0.04

0.03

Hastelloy B-2

Min. 

Balance 

26

2

        

Max. 

30

7

1

1

0.02

1

 

0.1

0.04

0.03

Hastelloy B Physical properties:

Density

9.24g/cm3

Melting point

1330-1380°C

 

Hastelloy B Alloy minimum mechanical properties in the room temperature:

Alloy state

Tensile strengthRm N/mm2

Yield strengthRP0.2N/mm2

ElongationA5 %

Hastelloy B

690

310

40

Characteristic:1. Control of iron and chromium content to a minimum to prevent the generation of β-phase Ni4Mo. 2. Excellent corrosion resistance of restore environment. 3. An excellent resist to concentration sulfuric acid medium and large number of non-oxidizing acid corrosion. 4. A very good resistance of chloride reduction of stress corrosion cracking (SCC). 5. Good corrosion resistance of various organic acids.Metallurgical structureHastelloy B-2 is the face-centered cubic lattice structure. By controlling the content of iron and chromium at the minimum to reduce the processing brittle, prevent Ni4Mo precipitation during 700-870 °C. Corrosion resistanceNi-Mo alloy Hastelloy B-2, the carbon and silicon content is extremely low, reducing the HAZ carbon and other impurities  precipitation, so the weld has sufficient corrosion resistance. Alloy Hastelloy B-2 in the reduction of medium with very good corrosion resistance, such as a various temperature and concentration of hydrochloric acid. In the middle of the concentration of sulfuric acid solution (or contain a certain amount of chloride ions) also has very good corrosion resistance. At the same time can be used to acetic acid and phosphoric acid environment. Alloy material suitable only in the metallurgical structure and pure crystal structure in order to have the best corrosion resistance.Applied field:Alloy Hastelloy B-2 with a wide range of applications in the field of chemical, petrochemical, energy manufacturing and pollution control , particularly in the sulfuric acid, hydrochloric acid, phosphoric acid, acetic acid, and other industries.

(Heat-resisting Superalloy Anticorrosion Alloy) Hot-rolled bar

Grade: 10-85mm

Application:  aviation, spaceflight, nuclear engrgy, weapons, heat-resitsting and anticorrosion parts for civil use; turbine disc, compressor disc, combustion chamber, blade

Advantage:Competitive price                   Good quality                   Timely delivery                   Perfect after-sales service

Superalloy